The density of the produced composites ranges from 400 to 1200 kg/m3 depending on formulation. The thermal conductivity increases proportionally with the density and ranges from 0.09 to 0.5 W/(m.K). The characterization of hygric behavior is based on the measurement of moisture buffer value (MBV) [1]. The hydric performances of the composites made of mineral binder goes from moderate (MBV around 1 g/(m².%RH)) to excellent (MBV > 2 g/(m².%RH)). The moisture buffer value of the paper granules -starch composite is also excellent (MBV > 2 g/(m².%RH))