Abstract
In this study, the microstructures and mechanical properties of 9%Cr reduced activation ferritic/martensitic (RAFM) steel friction stir welded joints were investigated. When a W-Re tool is used, the recommended welding parameters are 300 rpm rotational speed, 60 mm/min welding speed and 10 kn axial force. In stir zone (SZ), austenite dynamic recrystallization induced by plastic deformation and the high cooling rates lead to an obvious refinement of prior austenite grains and martensite laths. The microstructure in SZ contains lath martensite with high dislocation density, a lot of nano-sized MX and M3C phase particles, but almost no M23C6 precipitates. In thermal mechanically affect zone (TMAZ) and heat affect zone (HAZ), refinement of prior austenite and martensitic laths and partial dissolution of M23C6 precipitates are obtained at relatively low rotational speed. However, with the increase of heat input, coarsening of martensitic laths, prior austenite grains, and complete dissolution of M23C6 precipitates are achieved. Impact toughness of SZ at â20 °C is slightly lower than that of base material (BM), and exhibits a decreasing trend with the increase of rotational speed.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Chemistry
Authors
Chao Zhang, Lei Cui, Yongchang Liu, Chenxi Liu, Huijun Li,