| Article ID | Journal | Published Year | Pages | File Type |
|---|---|---|---|---|
| 7954742 | Procedia Structural Integrity | 2017 | 9 Pages |
Abstract
It is shown that the defect size is the first order parameter in terms of the fatigue resistance. Through the Kitagawa diagrams for as-built and heat treated samples, we quantify the improvement of the fatigue resistance due to the peak hardening treatment.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Chemistry
Authors
Julius N. Domfang Ngnekou, Yves Nadot, Gilbert Henaff, Julien Nicolai, Lionel Ridosz,