The interfacial reactions of continuous SiC fiber reinforced Ti-6Al-4V matrix composite (SiCf/Ti-6Al-4V composite) and continuous SiC fiber coated by C reinforced Ti-6Al-4V matrix composite (SiCf/C/Ti-6Al-4V composite) were investigated by using micro-beam electron diffraction (MBED) and energy disperse spectroscopy (EDS) on transmission electron microscopy (TEM). The sequence of the interfacial reactions in the as-processed and exposed at 900°C for 50h SiCf/Ti-6Al-4V composites can be described as SiC||TiC||Ti5Si3 + TiC||Ti-6Al-4V and SiC||TiC||Ti5Si3||TiC||Ti5Si3||TiC||Ti5Si3||Ti-6Al-4V, respectively. Additionally, both in as-processed and exposed composites, Ti3SiC2 and Ti3Si are absent at the interfaces. For the SiCf/C/Ti-6Al-4V composite exposed at 900 °C for 50 h, the sequence of the interfacial reaction can be described as SiC||C||TiCF||TiCC||Ti-6Al-4V before C coating is completely consumed by interfacial reaction. When interfacial reaction consumes C coating completely, the sequence of the interfacial reaction can be described as SiC||TiC||Ti5Si3||TiC||Ti-6Al-4V. Furthermore, in SiCf/C/Ti-6Al-4V composite, C coating can absolutely prevent Si diffusion from SiC fiber to matrix. Basing on these results, the model of formation process of the interfacial reaction products in the composites was proposed.
Related Topics
Physical Sciences and Engineering Materials Science Materials Science (General)
Authors
, , , , ,