Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7974321 | Materials Science and Engineering: A | 2018 | 8 Pages |
Abstract
The influence of intercritical tempering temperature on impact toughness of quenched and tempered 0.05C-5.42Mn medium-Mn steel was studied and compared with traditional tempering. The experimental steel had high hardenability because of high Mn-content. Lath-like α'-martensite without retained austenite was obtained over a wide range of quenching rate of 0.5-30 °C/s, and the quenched steel showed high strength but low impact toughness. On intercritical tempering at 625 °C and 665 °C, the impact toughness was enhanced, as compared to traditional tempering at 570 °C. The reversed austenite enriched with Mn and C formed between the martensite laths was the underlying reason for the increased absorbed crack propagation energy, and the ductile-brittle transition temperature (DBTT) was reduced because of increased stability of reversed austenite. Compared to the steel tempered at 625 °C, the steel tempered at 665 °C contained more reversed austenite, but the reversed austenite was less stable because of reduced enrichment of Mn and C. The enrichment or depletion of Mn and C in austenite and martensite was thermodynamically studied by DICTRA. In striking contrast to the steels tempered between 625 and 665 °C, twinned martensite was formed in the steel tempered at high temperature of 700 °C, and the steel exhibited impact toughness lower than the quenched steel.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
C. Sun, S.L. Liu, R.D.K. Misra, Q. Li, D.H. Li,