Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7977116 | Materials Science and Engineering: A | 2015 | 5 Pages |
Abstract
By Zn addition to the fusion zone, the interfacial intermetallic compounds (IMCs) of laser Al/steel joint changed from layered Fe2Al5 and needle-like FeAl3 to layered Fe2Al5âxZnx and dispersed FeZn10 with minor Al-rich amorphous phase. This resulted in an improvement in the joint strength and the change of failure mode.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
J. Yang, Y.L. Li, H. Zhang, W. Guo, Y. Zhou,