The effects of different additions of chromium (â¤8 at. %) on both the microstructure and room-temperature flow and fracture behavior of as-cast Fe30Ni20Mn35Al15 have been investigated. For â¤6 at. % Cr, the microstructure was lamellar consisting of (Ni, Al)-rich B2 and (Fe, Mn)-rich f.c.c. phases with most of the Cr residing in the f.c.c. phase, whilst the addition of 8 at. % Cr produced a more complex microstructure. The room-temperature elongation to failure at a strain rate of 5Ã10â4 s-1 increased with increasing Cr from 6.5% for the Cr-free material to ~18% at 6 at. % Cr, and then decreased dramatically for 8 at. % Cr to 6.3 %. Concomitantly, the yield stress decreased slightly from 820 to 679 MPa as the Cr content increased to 6 at. %, and then increased to 819 MPa for 8 at. % Cr. The addition of 6 at. % Cr also resulted in the complete suppression of the environmental embrittlement that is observed at slow strain rate at room temperature in the Cr-free alloy [1], i.e. at a strain rate of 3Ã10â6 sâ1 unalloyed Fe30Ni20Mn35Al15 showed only 0.7% elongation, whereas the alloy with 6 at. % Cr exhibited 18% elongation. The 6 at. % Cr modified alloy showed a similar temperature dependence of the yield strength as the Cr-free alloy [2], with the yield strength decreasing steadily to 150 MPa at 1000 K. Interestingly, the elongation to failure was largely independent of temperature for this alloy.
Related Topics
Physical Sciences and Engineering
Materials Science
Materials Science (General)
Authors
Fanling Meng, Jingwen Qiu, Ian Baker,