Abstract
Investment cast Ti45Al2Mn2Nb1B with fine lamellar microstructures was subject to fatigue crack propagation testing at 650 °C and a stress ratio of R = 0.1. The fracture surfaces were examined under SEM and the observed features are correlated with both stress intensity range (ÎK) and lamellar orientation. Translamellar fracture is primary fracture mode for most of the lamellar orientations. Interlamellar fracture is influenced by a combination of the ÎK and lamellar orientation. At low ÎK only the lamellar colonies with their lamellar interfaces almost perpendicular to the stress axis fractured via interlamellar fracture mode. At high ÎK interlamellar fracture can occur in lamellar colonies with any orientations.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
J. Yang, H. Li, D. Hu, M. Dixon,