Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7997908 | Journal of Alloys and Compounds | 2015 | 28 Pages |
Abstract
This work studied the effects of Cr content (0-0.67 wt%) and heat treatment on the microstructure evolution and high temperature (HT) tensile strength (350 °C) of the Fe-containing eutectic Al-Si alloy. For the HT strengths (350 °C), the UTSs of Al-Si alloys at T5 state are higher than T6 state correspondingly, both of which are progressively decreased with the Cr contents. For the elongation, the Al-Si alloys at T6 state have better plasticity than T5 state correspondingly. Comparably, the elongations remain stable at T5 state, and keep increasing at T6 state with the addition of Cr.109