Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7998958 | Journal of Alloys and Compounds | 2015 | 6 Pages |
Abstract
The effects of different adding methods of Li2CO3, H3BO3, Li2CO3-H3BO3 glass (B-Li glass) and Li2CO3-H3BO3 (LB) additives on the microstructure and microwave dielectric properties of 0.88(Mg0.4Zn0.6)2SiO4-0.12CaTiO3 (MZS-C) ceramics were investigated. Of all the adding methods, the addition of LB is the most effective way to lower the sintering temperature of MZS-C ceramics with good microwave dielectric properties. With LB addition, the MZS-C ceramics can be well sintered below 950 °C. The phase formation, microstructure, chemical compatibility with silver and microwave dielectric properties of MZS-C composite ceramics with LB addition were also systematically studied. The dielectric constant and QÃf value were related to the amount of the LB addition and sintering temperature. The near zero Ïf value can be obtained by adjusting the amount of LB addition. The MZS-C ceramics with 4.0 wt.% LB sintered at 950 °C/2 h exhibited excellent microwave dielectric properties of εr = 7.12, QÃf=28,600 GHz and Ïf = â6 ppm/°C. Meanwhile, the material was compatible with silver, which made it a promising candidate material for LTCC application.
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Wei Wang, Lingyu Li, Shaomei Xiu, Bo Shen, Jiwei Zhai,