In this paper, the microstructure and thermal treatment behavior of Zn-Al-SnO2/TiO2(Zn-Al-Sn/Ti) produced through co-deposition route was investigated. 7.0-13.0 wt% TiO2 and SnO2 was added to Zn-Al bath. Thermal treatment was done for 2 h at 200 °C, 400 °C and 600 °C. The ageing characteristics of the coated alloys were evaluated using (SEM/EDS) and XRD. The hardness and wear value of the thin film were examined with micro-hardness and UMT-2 sliding tester respectively. The corrosion properties were evaluated by linear polarization in 3.65% NaCl. From the result obtained, the coating exhibited good stability. The uniform distribution of the composites on the fabricated alloy and age-treatment were the major factor responsible for the mechanical and electrochemical improvement. The optimum value was obtained at Zn-Al-7Sn-Ti-0.3V-S for as-coated and Zn-Al-7Sn-Ti-0.3V-S at 400 °C for the thermal-aged samples. The stabilities in hardness and corrosion resistance against the working substrate were attributed to the formation of coherent and uniform precipitation in the metal lattice.
Related Topics
Physical Sciences and Engineering Materials Science Metals and Alloys
Authors
, , ,