Article ID Journal Published Year Pages File Type
8003510 Journal of Alloys and Compounds 2012 6 Pages PDF
Abstract
► CaO-B2O3-SiO2 glass was employed as the sintering aids. ► The sintering temperature of the composite ceramics was reduced to 850 °C effectively. ► Small dielectric loss of 2.0 × 10−3 was obtained. ► Relationships between glass additives and microstructure evolution were investigated. ► Relationships between glass additives and dielectric properties were discussed.
Related Topics
Physical Sciences and Engineering Materials Science Metals and Alloys