In order to illustrate the thermodynamic characteristics of arsenic during alkaline pressure oxidation leaching process of lead anode slime (NaNO3 as oxidant; NaOH as alkaline reagent), the Ï-pH diagrams of As-Na-H2O, N-H2O, As-N-Na-H2O systems at ionic mass concentration of 0.1 mol/kg and temperatures of 298, 373, 423 and 473 K were established according to thermodynamic calculation. The results show that the existence forms of arsenic are associated with pH value, which mainly exists in the forms of H3AsO4, H2AsO4â, HAsO42â, and As2O3 in lower pH region, while it mainly exists in the form of when pH>11.14. High alkali concentration and high temperature are advantageous to the arsenic leaching. The alkaline pressure oxidation leaching experiments display that the tendency of arsenic leaching rate confirms the thermodynamic analysis results obtained from the Ï-pH diagrams of As-N-Na-H2O system, and the highest leaching rate of arsenic reaches 95.85% at 453 K.
Keywords
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Yun-long HE, Rui-dong XU, Shi-wei HE, Han-sen CHEN, Kuo LI, Yun ZHU, Qing-feng SHEN,