Abstract
Pyrolusite was added in the bioleaching process to enhance the bio-oxidation process. Bioleaching tests at different dosages of pyrolusite ore, pH and inoculation amounts of Acidithiobacillus ferrooxidans were studied. The results showed that the time of the bio-oxidation process was decreased obviously and the arsenic leaching rate reached 94.4% after the bioleaching. The bio-oxidation of arsenopyrite and the effective extraction of manganese from pyrolusite were achieved by the bioleaching process. After bioleaching, the leaching rate of gold from the reaction residues reached 95.8% by cyanide leaching. In the bio-oxidation process, pyrolusite increased the redox potential of the solution to accelerate the bioleaching rate. The experiment showed that there were two reaction modes in the bioleaching process.
Related Topics
Physical Sciences and Engineering
Materials Science
Metals and Alloys
Authors
Xu ZHANG, Ya-li FENG, Hao-ran LI,