Abstract
Effects of mechanical alloying (MA) and titanium (Ti) content on the effective lattice parameter, crystallite size and lattice strain of the W-xTi (x=0.5, 1.0, 4.0 and 10.0Â wt% Ti) alloys were investigated. Using TOPAS 5 (Bruker AXS) software and Vegard's law, effective lattice parameters, aeff were determined from the X-ray diffraction (XRD) peak shift values at different MA durations and Ti contents. Lattice strain and crystallite sizes at varying MA durations and Ti contents were calculated by the Williamson-Hall method and Lorentzian rule using the TOPAS 5 (Bruker AXS) software. As expected, with increasing MA durations and Ti contents, effective lattice parameter and strain values increased and crystallite sizes decreased. Deviations of measured effective lattice parameter values from Vegard's law were analyzed. Negative deviations from the Vegard's law exist for the W-xTi (x=0.5, 1.0, 4.0 and 10.0Â wt% Ti) alloys MA'd for 10Â h and a maximum solubility of 11Â at% Ti was estimated for the W-10Â wt%Ti alloy MA'd for 10Â h. The smallest crystallite size of 2.21Â nm and the maximum strain of 4.57% were calculated for the W-4Â wt%Ti alloy MA'd for 20Â h.
Related Topics
Physical Sciences and Engineering
Materials Science
Nanotechnology
Authors
Hadi Jahangiri, M. Lütfi ÃveçoÄlu,