The degradation of the TBC columns increases with the duration of the 1200 °C heat-treatment. The interfacial Ca2Zr(Y)Si4O12 phase forms on an increasing amount of columns and is finally observed on all the columns. Interfacial phase formation is discussed and compared to other phase assemblages reported in the literature.