8031859 | Surface and Coatings Technology | 2011 | 6 Pages |
Abstract
⺠There was a metal Cr generated in the process of pretreatment. ⺠The Ni-P coating was amorphous, compact with good adhesion; the thickness was 50 μm. ⺠The corrosion potential of Ni-P coating shifted by 1090 mV positively. ⺠The corrosion current density of coated alloy decreased one order of magnitude. ⺠The salt spray test time of Ni-P coating was 210 h.