Abstract
SEM images illustrated the changing structures of PAA and PAAm. For PAA the deposited structure changed from a smooth film (20Â mm) to a film with individual droplets on the coated surface (100Â mm and 200Â mm), while for PAAm individual droplets can be seen at all distances. The ESD process with cascades of splitting droplets slows down for PAA after distances greater than 40Â mm. In contrast, the ESD process for PAAm is nearly stopped within the first flight distance of 20Â mm. Residual solvent analysis showed that most of the solvent evaporated within the first 20Â mm capillary-sample distance.