Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
8102610 | Journal of Cleaner Production | 2016 | 8 Pages |
Abstract
This study focuses on the recycling of stainless steel (SS) slags containing about 1.2 wt% of chromium (Cr). The selective recovery of Cr from SS slag by a hydrometallurgical method (alkaline pressure leaching) was investigated. Leaching experiments were carried out based on 24â1 factorial design of experiment (DOE) with the following parameters: NaOH concentration, temperature, leaching time, and mechanical activation (MA). Results show that temperature and MA are the most influencing factors for an enhanced Cr leaching. The maximum Cr leaching was 46% at 1 M NaOH, 240 °C, 6 h, MA 30 min, while the matrix material was dissolved only to a limited extent (Al 2.88%, Si 0.12%, Ca 0.05%). After Cr leaching followed by alkali washing, a carbonation treatment is proposed to stabilize the remaining Cr in the matrix material and make the subsequent recycling of the matrix material as a construction material possible.
Related Topics
Physical Sciences and Engineering
Energy
Renewable Energy, Sustainability and the Environment
Authors
E. Kim, J. Spooren, K. Broos, P. Nielsen, L. Horckmans, R. Geurts, K.C. Vrancken, M. Quaghebeur,