Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
8155131 | Journal of Magnetism and Magnetic Materials | 2016 | 16 Pages |
Abstract
The aim of this work is to investigate the effect of very fine grain sizes on the spinodal decomposition in the Alnico system. Commercial Alnico 5 was melted and melt-spun with varying copper wheel speeds, which led to a grain size of 1-2 µm. This value was further reduced to sub-micrometer size by a small addition of Boron (1 at%). The spinodal decomposition was induced through a two-step annealing treatment under magnetic field in the range of 600-900 °C. It was found that the size of the spinodal structures is not influenced much by increased wheel speeds but becomes smaller with the addition of Boron. However, the difference in coercivity between the samples with and without Boron is only 50 Oe (4 kA/m). To study the influence of the annealing treatment two sets of samples are compared, one with the highest coercivity (366 Oe/29 kA/m) and the other one with lower coercivity (180 Oe/14.5 kA/m). We found with Scanning transmission electron microscopy Energy-dispersive X-ray spectroscopy (STEM EDX) a much sharper chemical interface between the α1 and α2 precipitates in the former sample, which we attribute to be the main reason for the higher coercivity.
Related Topics
Physical Sciences and Engineering
Physics and Astronomy
Condensed Matter Physics
Authors
Konrad Löwe, Michael Dürrschnabel, Leopoldo Molina-Luna, Rajasekhar Madugundo, Bianca Frincu, Hans-Joachim Kleebe, Oliver Gutfleisch, George C. Hadjipanayis,