Abstract
The magnetic domain wall energy density σW of a Ni/Co superlattice possessing perpendicular magnetic anisotropy was determined using the magnetic domain theory derived by Kooy and Enz (1960). To determine σW, we obtained the saturation magnetization, magnetic domain period, and perpendicular magnetic anisotropy energy by individual measurements. Using the magnetic domain period and the ferromagnetic layer thickness, we first determined the dipolar length. The estimated dipolar length was about 15-25 nm, which is in good agreement with the change in the magnetization curve with the ferromagnetic layer thickness. By using the dipolar length and saturation magnetization, the σW was calculated to be 4-7 erg/cm2.