Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
8156751 | Journal of Magnetism and Magnetic Materials | 2014 | 5 Pages |
Abstract
To enhance coercivity and reduce the rare-earth consumption of Nd-Fe-B sintered magnets simultaneously, low melting point Dy69Ni31 (at%) powders are introduced into a slightly off-stoichiometric Nd2Fe14B (2:14:1 phase) (Pr, Nd)12.36FebalB6.09 (at%) starting magnet. Because of insufficient rare-earth element, the starting magnet possesses discontinuous intergranular grain boundaries (GBs) that cannot decouple the 2:14:1 phase grains well, hence leading to a low coercivity of only 9.53Â kOe. The Dy69Ni31 additive provides extra rare-earth that improves the liquid-phase sintering with the formation of continuous intergranular GBs, accompanied by the diffusion of Dy towards surface region of the 2:14:1 phase grains. A significant increment in coercivity of 6.25Â kOe is realized with a slight reduction in remanence by â3.0% per unit at% Dy. Satisfactory magnetic performance with (BH)max=47.49 MGOe, Br=13.92 kGs and Hcj=13.93Â kOe, is obtained in the magnet containing only 12.92 at% rare-earth elements, in which 0.68 at% Dy is included. It combines advantages of the modification of intergranular GBs and the formation of a magnetically hardening shell surrounding 2:14:1 phase grains, which can be a promising approach to fabricate low rare-earth and high performance Nd-Fe-B magnets for mass production.
Related Topics
Physical Sciences and Engineering
Physics and Astronomy
Condensed Matter Physics
Authors
Xiaolian Liu, Xuejiao Wang, Liping Liang, Pei Zhang, Jiaying Jin, Yujing Zhang, Tianyu Ma, Mi Yan,