| Article ID | Journal | Published Year | Pages | File Type | 
|---|---|---|---|---|
| 8158789 | Journal of Magnetism and Magnetic Materials | 2013 | 4 Pages | 
Abstract
												⺠When Cr is 8 at%, after 60 h milling, D03 superlattice appeared. And exothermic peak appears at 685 K. ⺠With increasing Cr content, Ms decreases from 145 to 99 emu/g; μⳠis larger than the others at low frequency. ⺠The minimum reflectivity is â15.5 dB at 8.5 GHz for Cr content is 8 at% when thickness is 2 mm. ⺠The amorphous Fe78.5Si13.5Cr8 alloy can be applied as electromagnetic wave absorber.
											Keywords
												
											Related Topics
												
													Physical Sciences and Engineering
													Physics and Astronomy
													Condensed Matter Physics
												
											Authors
												B.F. Zou, T.D. Zhou, J. Hu, 
											