Abstract
We report here the effect of Eu2+ concentration in KCa0.8Sr0.2I3:Eu2+ single crystal scintillators. KCa0.8Sr0.2I3:Eu2+ single crystals doped with 0.5, 1, 3, 5, and 7 mol% Eu2+ were grown by the Bridgman method. The effects of varying Eu2+concentration and crystal volume on the scintillation properties, including light yield, energy resolution, nonproportionality, scintillation decay time and afterglow level, were systematically investigated. For 5 mmÃ5 mmÃ5 mm samples, the best light yield of 86,000±4000 photons/MeV was achieved with a content of 5 mol% Eu2+; its energy resolution of 2.5% at 662 keV was comparable to that of LaBr3:Ce3+ and SrI2:Eu2+. With larger samples of about 2.2 cm3, the best performances achieved were for 3 mol% Eu2+ concentration, i.e. a light yield of 76,000±4000 photons/MeV and an energy resolution of 3% at 662 keV. A direct correlation between nonproportionality and Eu2+ concentration was found. A continuous lengthening of scintillation decay time and x-ray induced afterglow level with increasing Eu2+ concentration was observed. The self-absorption effect was evaluated by using the Stokes shift and the temperature dependence of the photoluminescence decay (PL) of the Eu2+ centers. The sample with the highest dopant concentration had more severe temperature quenching of the Eu2+5d-4f emission than the sample with the lowest dopant concentration, which could be ascribed to the thermally activated concentration quenching.
Related Topics
Physical Sciences and Engineering
Physics and Astronomy
Instrumentation
Authors
Yuntao Wu, Mariya Zhuravleva, Adam C. Lindsey, Merry Koschan, Charles L. Melcher,