Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
9717369 | Composites Science and Technology | 2005 | 11 Pages |
Abstract
Fractographic evaluations carried out under scanning electron microscope (SEM) confirm the quantitative characterisation obtained from static and dynamic mechanical analysis. The Arrhenius relationship has been used to calculate the activation energy of the glass transition of the polyester. The highest activation energy was found in hybrid composite with volume ratio of banana and sisal as 3:1. A master curve was constructed based on time-temperature superposition principle. Finally, the experimental results were compared with theoretical predictions.
Related Topics
Physical Sciences and Engineering
Engineering
Engineering (General)
Authors
Maries Idicula, S.K. Malhotra, Kuruvilla Joseph, Sabu Thomas,