Most of ceramic oxides showed good chemical stability on chlorine, oxygen and uranyl chloride from thermodynamic calculation results. On the other hand, from corrosion test result, silicon nitride, mullite (Al6Si2O13) and cordierite (Mg2Al3(AlSi5O18)) have a good corrosion resistance which is corresponding to 0.1Â mm/y or less. No cracks on the materials were observed and flexural strength did not drop remarkably after 480Â h corrosion testing in molten salt under Cl2-O2 atmosphere.