Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
9834090 | Journal of Magnetism and Magnetic Materials | 2005 | 12 Pages |
Abstract
Powder mixtures of (FeyN)x and (Al2O3)1âx or (SiO2)1âx with x=0.2 and 0.6 and y=3.8 have been ball milled for 4, 8, 16, 32, 64, and 128 h and their magnetic properties and Mössbauer spectra have been measured. The 5 and 295 K saturation magnetizations decrease with increasing milling time as a result of decreasing particle sizes. Fits with the Langevin function of the field dependence of the magnetization yield particle sizes that are slightly smaller than those determined from a Scherrer analysis of the broadening of the X-ray diffraction peaks. The Mössbauer spectra have been fit with a distribution of hyperfine fields between 0 and 40 T and the peaks in the distribution assigned to the different iron nitride phases present in the nanocomposites. This analysis of the Mössbauer spectra indicates that the γâ²-Fe4N phase present in FeyN is transformed into ε-Fe3+xN and α-iron by the milling process. The weighted average field decreases and the weighted average isomer shift increases with milling time, as expected for the simultaneous effects of size reduction, the above phase transformation, and mixing with the oxides. A peak in the hyperfine field distribution at 4 T indicates the presence of small superparamagnetic particles, a presence which is also confirmed by the temperature dependence of the Mössbauer spectra and the failure of the magnetization to saturate even at applied fields of 5.5 T.
Related Topics
Physical Sciences and Engineering
Physics and Astronomy
Condensed Matter Physics
Authors
Fernande Grandjean, Raphaël P. Hermann, Gary J. Long, Sanjay R. Mishra,