Article ID Journal Published Year Pages File Type
9952575 Wear 2018 34 Pages PDF
Abstract
Results have shown that for full HCP phase coatings (Ag67Al33), wear rates are lowest, with no adhesive wear and good surface sulphidation resistance, though with some proclivity to oxidation, coupled with a moderate increase in the electrical contact resistance.