Article ID Journal Published Year Pages File Type
10378163 Journal of Colloid and Interface Science 2005 6 Pages PDF
Abstract
ZnO nanoparticles with spherical morphology and narrow size distribution were obtained by calcination of Zn(OH)2 nanoparticles, which were prepared in a polyethylene glycol mono-4-nonylphenyl ether (NP-5)/cyclohexane reverse micellar system and incorporated into polyurea (PUA) via an in situ polymerization of hexamethylene diisocyanate (HDI). The resulting ZnO nanoparticles demonstrated a near-UV emission and a green emission, the intensity ratio of which depended on calcination conditions. For the nanoparticles studied, the calcination atmosphere influenced remarkably the photoluminescence properties such as intensity ratio of the near-UV emission to green emission, rather than the size, morphology, and crystallinity of the ZnO nanoparticles. The green emission decreased by calcination in O2 flow but increased by calcination in N2 flow, as compared with the case calcined in air flow. This finding suggests that the green emission is enhanced with the increase of the number of oxygen vacancies of the ZnO nanoparticles and thus the photoluminescence properties of the nanoparticles were successfully controlled by the calcination condition, without changing the size and morphology.
Related Topics
Physical Sciences and Engineering Chemical Engineering Colloid and Surface Chemistry
Authors
, ,