Abstract
Heat loads expected for VDEs in ITER were applied in the neutral beam facility GLADIS at IPP Garching. Several ∼3 mm thick rolled pure W and W-1 wt% La2O3 plates were exposed to pulsed hydrogen beams with a central heat flux of 23 MW/m2 for 1.5-1.8 s. The melting thresholds are determined, and melt layer motion as well as material structure evolutions are shown. The melting thresholds of the two W grades are very close in this experimental setup. Lots of big bubbles with diameters from several μm to several 10 μm in the re-solidified layer of W were observed and they spread deeper with increasing heat flux. However, for W-1 wt% La2O3, no big bubbles were found in the corrugated melt layer. The underlying mechanisms referred to the melt layer motion and bubble issues are tentatively discussed based on comparison of the erosion characteristics between the two W grades.
Related Topics
Physical Sciences and Engineering Energy Nuclear Energy and Engineering
Authors
, , , , , , ,