Abstract

Pd deposits are obtained by applying −1.92 mA cm−2 during 180 min, employing 0.06 M PdCl2 + 1 M HCl and 0.06 M PdCl2 + 28% NH3 solutions. Some features on Pd depositions using x M PdCl2 + 1 M HCl (x = 0.130, 0.060, 0.030, 0.025, 0.020 and 0.010) solutions are detailed. Based on roughness factor (S) and deposition efficiency (ɛPd) values, Pd deposition is more efficient using PdCl2 + 1 M HCl than PdCl2 + 28% NH3 (ɛPd = 99%, S = 6 in 1 M HCl vs. ɛPd = 17%, S = 3 in 28% NH3). A highly rough Pd deposit (S = 357) is obtained, by applying −1.92 mA cm−2 during 180 min, using a 0.020 M PdCl2 + 1 M HCl solution.

► Assisted Pd electrodeposition is more efficient in HCl than in NH3 solutions. ► Highly rough Pd deposits are obtained using 0.030 M PdCl42− + 1 M HCl. ► Pd deposition efficiencies are affected by PdCl2 concentration. ► Modified Pd membranes are usable for electrochemical assisted hydroconversion.

Related Topics
Physical Sciences and Engineering Chemistry Electrochemistry
Authors
, , , , ,