Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1462987 | Ceramics International | 2011 | 5 Pages |
Abstract
Powders of Al4C3 and SiC were combined by high-energy milling to produce Al4SiC4, Al4SiC4 + 30 vol.% TiC, and Al4SiC4 + 30 vol.% WC. Five different temperatures were used to hot press the constituents. XRD, SEM, relative density, and hardness measurements showed that formation of single-phase Al4SiC4 occurred at 1450 °C and full densification (99%) was achieved at 1500 °C. Both of these temperatures are lower than previously reported. Adding TiC and WC increases hardness, while WC improves densification (99.5%).
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
Osama Gaballa, Bruce Cook, Alan Russell,