Article ID Journal Published Year Pages File Type
1483446 Journal of Non-Crystalline Solids 2010 7 Pages PDF
Abstract
Samples of Fe78B13Si9 (Metglas 2605 TCA) and Fe77Cr2B16Si5 (Metglas 2605 S3A) were exposed to pulsed excimer laser irradiation at repetition rates of 15, 25 and 50 Hz. The occurrence of out-of-plane magnetic anisotropy, changes in the average hyperfine magnetic field and width of the hyperfine field distribution were evidenced by transmission Mössbauer spectroscopy. The variation of the recoilless fraction with laser processing parameters was derived from the simultaneous recording of Mössbauer spectra using a stainless steel etalon as a dual absorber. Conclusions on the onset of long-range magnetic order were formulated.
Related Topics
Physical Sciences and Engineering Materials Science Ceramics and Composites
Authors
,