Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1565572 | Journal of Nuclear Materials | 2013 | 12 Pages |
In the article presented are the results of post-irradiation tests of helium bonded fuel pins with mixed mononitride fuel (U0.55Pu0.45)N and (U0.4Pu0.6)N having 85% density irradiated in BOR-60 reactor. Achieved maximum burn-up was, respectively, equal to 9.4 and 12.1 at.% with max linear heat rates 41.9 and 54.5 kW/m. Maximum irradiation dose was 43 dpa. No damage of claddings made of ChS-68 steel (20% cold worked) was observed, and ductility margin existed. Maximum depth of cladding corrosion was within 15 μm. Swelling rates of (U0.4Pu0.6)N and (U0.55Pu0.45)N were, respectively, ∼1.1% and ∼0.68% per 1 at.%. Gas release rate did not exceed 19.3% and 19%. Pattern of porosity distribution in the fuel influenced fuel swelling and gas release rates.