Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1568970 | Journal of Nuclear Materials | 2008 | 4 Pages |
Abstract
Reaction kinetic analysis was used to estimate the damage evolution in window materials of 800Â MWth accelerator driven system (ADS). Parameters were fitted to F82H of the STIP-II experiment at 673Â K and EC316LN of the STIP-I experiment at 626Â K. In F82H, the concentration of bubbles was almost constant and the bubble size increased, while the concentration of interstitial type dislocation loops increased and their size was constant between 2.1Â ÃÂ 10â3 and 210Â dpa. EC316LN showed almost the same behavior. Swelling increased almost linearly with irradiation dose above 0.21Â dpa between 673Â K and 773Â K.
Related Topics
Physical Sciences and Engineering
Energy
Nuclear Energy and Engineering
Authors
T. Yoshiie, Q. Xu, K. Sato, K. Kikuchi, M. Kawai,