Abstract

The diffusivity of oxygen in liquid lead and lead–bismuth eutectic (LBE) alloy was measured by a potentiostatic method and is given by log(DOPb/cm2s-1)=-2.554-2384/T(±0.070), 818–1061 K, and log(DOLBE/cm2s-1)=-0.813-3612/T(±0.091), 811–980 K. The activity of oxygen in lead and LBE was determined by coulometric titration experiments. Using the measured data, the standard free energy of dissolution of oxygen in liquid lead and LBE was derived and is given byGO(Pb)xs=-121349+16.906T(±560)J(gatomO)-1,815–1090K,GO(LBE)xs=-127398+27.938T(±717)J(gatomO)-1,812–1012K.Using the above data, the Gibbs energy of formation of PbO(s) and equilibrium oxygen pressures measured over the oxygen-saturated LBE alloy, the solubility of oxygen in liquid lead and LBE were derived. The solubility of oxygen in liquid lead and LBE are given by log(S/at.%O) = −5100/T + 4.32 (±0.04), 815–1090 K and log(S/at.%O) = −4287/T + 3.53 (±0.06), 812–1012 K respectively.

Keywords
Related Topics
Physical Sciences and Engineering Energy Nuclear Energy and Engineering
Authors
, , ,