Article ID Journal Published Year Pages File Type
179806 Electrochemistry Communications 2012 4 Pages PDF
Abstract

We have used 1.5 wt.% of nanodiamonds having three different sizes such as 5, 50 and 250 nm for making the hybrid active layer. As the nanodiamond size increased, the root mean square (rms) roughness also increased in the film. The film with nanodiamond has a higher absorption intensity than the P3HT:PCBM film. The power conversion efficiency (PCE) of the device has improved from 1.8% to 2.4%, as a result of increased current density for P3HT:PCBM mixed with nanodiamond having 50 nm.

► A novel technology for preparing hybrid diamond organic films is presented. ► The hybrid light-activated P3HT/PCBM/ nanodiamond is performed. ► A highly absorption with high hybrid nanodiamonds of 50 nm is achieved. ► Enhancing current density of photovoltaic device are obtained.