Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
180573 | Electrochemistry Communications | 2010 | 5 Pages |
Abstract
Single phase LiCr0.2Ni0.4Mn1.4O4 spinel has been synthesized by a simple sucrose assisted combustion method that yields highly crystalline homogeneous sub-micrometric samples (650 nm). The LiCr0.2Ni0.4Mn1.4O4, with capacity retention of 92% at 60 C discharge rate, shows the highest rate capability among LiNi0.5Mn1.5O4-type cathodes. It delivers very high-power (34.8 kW kg−1 at 60 C). Studies developed at 55 °C demonstrate that LiCr0.2Ni0.4Mn1.4O4 retains huge rate capability and large cycleability at high temperature.
Related Topics
Physical Sciences and Engineering
Chemical Engineering
Chemical Engineering (General)
Authors
Mohamed Aklalouch, José Manuel Amarilla, Rosa M. Rojas, Ismael Saadoune, José María Rojo,