Abstract
⺠La0.6Ca0.4Fe0.8Ni0.2O3 electrodes were produced at a range of temperatures. ⺠The fully reacted powder is obtained at low temperature (600 °C). ⺠Symmetrical cells were produced by spray technique. ⺠Porous microstructure is obtained at low sintering temperatures (800 °C). ⺠Overall processing route is optimized with no detrimental effects on performance.