Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
6705226 | Composite Structures | 2016 | 11 Pages |
Abstract
Glass-fibre epoxy composite, GLARE, and heated GLARE samples have been thermal cycled for 4000, 8000 and 12,000 cycles with temperature differences of 120 °C. The interlaminar shear strength (ILSS) increased by 6.9% after 8000 cycles for the glass-fibre epoxy composite material compared to the non-cycled samples. The GLARE samples showed a maximum ILSS increase of 4.2% after 12,000 cycles. However, the heated GLARE samples showed a continuous decrease of the ILSS with a maximum decrease of 7.8% after 12,000 cycles.
Related Topics
Physical Sciences and Engineering
Engineering
Civil and Structural Engineering
Authors
Bernhard Müller, Michiel Hagenbeek, Jos Sinke,