Abstract
⺠PGP was prepared at high arc current and large anode diameter; MWNT was prepared at low arc current small anode diameter. ⺠PGP was prepared at high arc current and large anode diameter; MWNT was prepared at low arc current small anode diameter. ⺠Relatively high ratio of carbon ions to carbon radicals contributes to the formation of PGP. ⺠Relatively low ratio of carbon ions to carbon radicals leads to the formation of MWNT.
Related Topics
Physical Sciences and Engineering
Engineering
Electrical and Electronic Engineering
Authors
Feng Liang, Tasuku Shimizu, Manabu Tanaka, Sooseok Choi, Takayuki Watanabe,