Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7903891 | Journal of Non-Crystalline Solids | 2013 | 8 Pages |
Abstract
⺠Pd41.75Ni41.75P17.5 BMGs were annealed to allow a spinodal mechanism to take place. ⺠The spinodal microstructures as a function of annealing times were determined. ⺠The lower bound of the duration of the spinodal decomposition at a temperature of â 625 K is about 200 s. ⺠The time constant R of the spinodal decomposition at a temperature of â 625 K is ~ 0.002 sâ 1.
Related Topics
Physical Sciences and Engineering
Materials Science
Ceramics and Composites
Authors
S. Lan, M.T. Lau, H.W. Kui,