Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7965301 | Journal of Nuclear Materials | 2015 | 6 Pages |
Abstract
Flexible flame-retardant composites were prepared using high-functional methyl vinyl silicone rubber matrix with B4C, hollow beads, and zinc borate (ZB) as filler materials. As filler content increased, the tensile strength, elongation, and tear strength of the composites initially increased and then decreased. The shore hardness of the composites increased with increasing filler content with a maximum value of 30 HA. The heat insulation properties of the composites with hollow beads were higher than that of the ordinary composites with the same filler mass fraction. When ZB content exceeded 12Â wt%, the limit of oxygen index of the composites was higher than 27.1%. With Am-Be neutron as the test radiation source, the transmission of neutron for a 2Â cm sample was only 47.8%. Powder surface modification improved the mechanical properties, thermal conductivity, flame retardancy, and neutron shielding performance of the composites, but did not affect shore hardness.
Related Topics
Physical Sciences and Engineering
Energy
Nuclear Energy and Engineering
Authors
Hao Chai, Xiaobin Tang, Minxuan Ni, Feida Chen, Yun Zhang, Da Chen, Yunlong Qiu,