Ni foil is used as interlayer to join Zircaloy-4 by transient liquid phase bonding. The Zoneβâα is formed in the joints and its width increases with temperature. The formation of Zoneβâα is controlled by both bonding temperature and Ni concentration. The Zoneβâα is mainly composed of primary Zr phase and eutectic Zr(Zr2Ni) structure. The micro-hardness of the joints mainly depends on the precipitates and the size of α-Zr phase. The non-planar bonding interfaces are developed in the joints when the bonding temperature above 960 °C. Resulting from the non-planar bonding interfaces, the maximum shear strength of the joints is 358 ± 19 MPa.