Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
1287715 | Journal of Power Sources | 2013 | 5 Pages |
•Li3V2(PO4)3/C has been firstly synthesized by an in-situ copolymerization method.•The polyacrylamide as carbon source is firstly introduced into Li3V2(PO4)3/C system.•The chelating reagent and copolymerization method is firstly combined.•The Li3V2(PO4)3/C exhibits excellent cyclic performance at high discharge rates.
High rate cathode Li3V2(PO4)3/C with an excellent electrochemical performance has been successfully synthesized via an in-situ copolymerization method. The synthesized Li3V2(PO4)3/C composite exhibits an extraordinary reversible discharge capacity of 103.1 mAh g−1 at 50 C discharge rate. In addition, there are no obvious capability fade after 100 cycles. The carbon from pyrolysis of polyacrylamide obtained from the in-situ copolymerization reaction is believed acting a critical role in acquiring such high performances.