The lithium, as well as the TM amount, found on the anode, is directly correlated to the applied upper cut-off voltage (4.6, 4.7, 4.8 and 4.9 V) showing more deposition of Li and TMs at elevated voltages. While 7Li shows a more homogeneous pattern, the TM distribution is inhomogeneous but showing a similar pattern for all TMs of the same sample. An unequal pressure distribution, resulting in a nonparallel electrode alignment, on the electrode stack is identified to be responsible for the inhomogeneous TM deposition pattern. This uneven electrode orientation results in different diffusion pathways for the TM migration with regard to the spatial distances.