Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7736076 | Journal of Power Sources | 2014 | 5 Pages |
Abstract
Subsequently, the nanometer 4BS as additive is added to positive paste of lead-acid battery. When the batteries are tested galvanostatically between 1.75 V and 2.42 V at 0.25 C charge and 0.5 C discharge rates at room temperature. The ratio of adding nanometer 4BS is 0%, 1% and 4% and the initial discharge specific capacities are 60 mAh gâ1, 65 mAh gâ1 and 68 mAh gâ1. After 80 cycles, the initial discharge capacity of positive active material with 1% nanometer 4BS decreased less than 10%, while adding 4% nanometer 4BS, the initial discharge capacity doesn't decrease obviously.