The Ce2Ni7-type (hexagonal, 2H) single phase La1.6Mg0.4Ni7 alloy has been obtained by annealing the induction melting as-cast sample at 1223 K for 12 h. The relationship between phase structural stability and volume change rate of the three kinds of slabs in Ce2Ni7-type structure is studied. It is found that the volume change rate of Mg-containing [La1.22Mg0.78Ni4] slab after hydrogenation/dehydrogenation is larger than that of [LaNi5] I (outer) and [LaNi5] II (inner) slabs, and the consecutive cell volume change of [La1.22Mg0.78Ni4] slab ultimately results in the decomposition of Ce2Ni7-type phase La1.6Mg0.4Ni7 to amorphous La and Mg phases, nanocrystalline Ni, and CaCu5-type LaNi5 phases, as well as the reduction of electrochemical discharge capacity. Electrochemical studies show that the single phase alloy electrode possesses good discharge capacity (400 mAh gâ1) and cycling stability (84.2% after 100 cycles). The improvement in phase structure stability and the cycling stability of the superlattice structure alloys can be achieved by inhibiting the significant volume change of Mg-containing slabs during hydrogenation/dehydrogenation.
Related Topics
Physical Sciences and Engineering
Chemistry
Electrochemistry
Authors
Lu Zhang, Shumin Han, Da Han, Yuan Li, Xin Zhao, Jingjing Liu,