Article ID | Journal | Published Year | Pages | File Type |
---|---|---|---|---|
7740474 | Journal of Power Sources | 2013 | 8 Pages |
Abstract
In order to improve the performance of the Li[Ni0.5Co0.2Mn0.3]O2, a novel spherical Li[Ni0.5Co0.2Mn0.3]O2-Li2MnO3 core-shell composite has been successfully synthesized by a simple sol-gel deposition method. It is found that the core-shell composite consists of Li[Ni0.5Co0.2Mn0.3]O2 as the core and Li2MnO3 as the outer shell according to examination by scanning electron microscope (SEM) with energy dispersive X-ray spectroscopy (EDXS) and X-ray diffraction (XRD). The core-shell composite delivers a high capacity of 180.4 mAh gâ1 at a rate of 0.1 C in the voltage range of 2.0-4.4 V. Most importantly, the core-shell composite exhibits excellent capacity retention of 98.8% after 200 cycles at a rate of 0.5 C, and 93.8% capacity retention after 100 cycles at a rate of 5 C at room temperature. When cycled at an elevated 55 °C, the prepared sample exhibits only 2.3% capacity loss after 100 cycles. Meanwhile, the core-shell composite shows significantly improved thermal stability relative to that of the pristine Li[Ni0.5Co0.2Mn0.3]O2. The improved stability of the core-shell composite is ascribed to the stable Li2MnO3 outer shell, which can prevent the Li[Ni0.5Co0.2Mn0.3]O2 core from direct contact with the electrolyte, and the core material could operate with no risk of structural disruption at high voltages and high temperatures.
Related Topics
Physical Sciences and Engineering
Chemistry
Electrochemistry
Authors
Xiukang Yang, Xianyou Wang, Liang Hu, Guishan Zou, Shaojuan Su, Yansong Bai, Hongbo Shu, Qiliang Wei, Benan Hu, Long Ge, Di Wang, Li Liu,