⺠LSCO4 oxide is chemically compatible with CGO and LSGM electrolyte at 1100 °C. ⺠A low electrode polarization resistance of 0.21 Ω cm2 is achieved at 750 °C. ⺠The low ASR exhibits high electrochemical activity at intermediate temperature range. ⺠The single cell shows a maximum cell power density of 515 mW cmâ2 at 750 °C. ⺠The LSCO4-CGO composite oxides are one of promising cathode candidates for IT-SOFCs.